Description
-
Conforms to ASTM E 139
-
Stable & Reliable performance
-
PC based data acquisition system
Application
The Impression Creep Test Rig is designed to provide solution for maintaining constant loads for long term creep & stress rupture testing applications of metallic materials in accordance with ASTM E 139. These tests can run from only a few hours up to and exceeding 10000 hours. The long duration of these tests makes the lever arm loading system with dead weights.
Conforms to ASTM E 139
Stable & Reliable performance
PC based data acquisition system
Capacity -100 kg
Loading arrangement-manual by dead weight in steps of 0.10kg,
0.25kg, 0.50kg & 1 kg
Indenter material-Tungsten carbide
Indenter dimensions-1.0, 1.5 & 2.0mm diameter
Specimen dimension-15mm x 20mm square (approx)
LVDT -0-5mm range with resolution of 1 micron
Heating arrangement-Cylindrical furnace
Temperature range-6000C
Vacuum level-Vacuum of 2E-6bar or better
Temperature accuracy-±10C
Deflection sensor-LVDT
Data output-Tabular and graphical for depth of indentation
versus time, creep strain versus time, creep
strain rate versus time, creep strain rate versus
strain.
Reviews